Causes of Cracks in Ceramic Fibre Paper Blanks and Solutions

2026-11-04 Visits:40

(1) Causes

1. Certain specifications of the ceramic fibre wadding currently in production remain unclear to the paper-making line

① Fibre diameter

② Aluminium content

2. Cost reduction and quality improvement are at odds with one another

① In order to reduce costs, the granulated wadding frequently changes raw materials and formulations, resulting in the paper-making line for ceramic fibre paper not yet having clear specifications for the paper-making wadding (the blowing line has altered the stability of certain specifications of the fibre wadding)

Paper production lines are therefore forced to proceed by trial and error.

Remedial Measures

Stabilise the specifications and quality of the fibre batt to ensure that the ceramic fibre paper production line has a clear understanding of its specifications and composition.

(II) Pulping Section

1. Inappropriate raw material proportions.

2. Excessive use of aluminium sulphate.

3. Pulp is too coarse.

4. High levels of sludge balls and non-fibrous matter, or an excessively high bulk density of the paper sheet.

5. Unsuitable circulating water quality (pH value should be below 7; must not contain large quantities of microorganisms).

6. Typically occurs during periods of higher ambient temperatures (after the Minor Heat solar term in summer).

7. Mismatched speed ratios.

8. Ambient temperature too low when producing HB-type paper

9. Concentration too high or too low

Remedial Measures

1. Ensure appropriate raw material proportions

2. Ensure appropriate addition of aluminium sulphate

3. Extend the beating time; the pulp should not be too coarse. For sizes of 4 mm and above, aim for a finer consistency wherever possible; it must not be too coarse.

4. An excessive amount of non-fibrous material (slag balls) within the ceramic fibre paper sheet causes uneven interlacing of fibres; ensure frequent slag removal and board insertion.

5. When preparing the pulp, add an appropriate strong acid agent to the tank and maintain good circulating water quality (pH below 7 is suitable; there must be no large quantities of microorganisms);

6. Increase the dosage of wet-strength agent, but avoid excessive amounts to prevent excessive foaming (to enhance the retention of binder in the wet green body after dewatering);

7. Ensure the concentration is appropriate and stable; it should not be too high or too low.

8. Add an appropriate amount of high-alumina ceramic fibre wool (with small fibre diameter and high aluminium content) to improve tensile strength, organic content and flexural strength.