As a new type of inorganic non-metallic material, ceramic fibre paper has become a core thermal insulation material in sectors such as aerospace, metallurgy and chemical engineering, and electronic packaging, thanks to its low thermal conductivity, high flexibility and thermal shock resistance. Its manufacturing process integrates nanotechnology, fluid mechanics and precision moulding techniques, forming a complete technological chain ranging from the nanoscale processing of raw materials to the functionalisation of the finished product. Today, Mu Yi provides an in-depth analysis of its technical principles and key process control points across four major dimensions: raw material pre-treatment, fibre forming, paper-base construction, and post-treatment reinforcement.
I. Raw Material Pre-treatment: Quantum-level Control of Nanoscale Sol-Gel Systems
1. Preparation of Nanopowders
Core Raw Materials: Primarily Al₂O₃ (≥45%) and SiO₂ (≥50%), supplemented by nucleating agents such as ZrO₂ (≤3%) and Cr₂O₃ (≤2%)
Preparation Process:
Wet ball milling: Using zirconia beads at a speed of 400 rpm and a ball-to-material ratio of 5:1, milled until D50 < 100 nm
Ultrasonic Dispersion: Treated for 30 minutes at a frequency of 20 kHz to eliminate agglomeration and increase the specific surface area to 200–300 m²/g
Quality Standards:
Fe₂O₃ content ≤ 0.5% (to prevent phase transformation at high temperatures)
Total Na₂O + K₂O ≤ 0.3% (to reduce the risk of glass phase precipitation)
2. Construction of the sol–gel system
pH control: within the range of 3.5–4.0 to promote the hydrolysis and condensation of Al³⁺ and Si⁴⁺ to form a three-dimensional network structure
Addition of dispersant: 0.5–1.0 wt% polyvinyl alcohol (PVA) to reduce surface tension to 30–35 mN/m
Seed Induction: Introduction of 1–3 wt% nano-ZrO₂ seeds to induce the oriented growth of α-Al₂O₃ crystal nuclei
Rheological Properties: Monitored in real time using a rotational viscometer to maintain sol viscosity at 800–1200 mPa·s
II. Fibre Formation: Synergistic Process Combining Electrospinning and Centrifugal Spinning
1. Electrospinning Technology
Process Parameters:
Voltage gradient: 15–25 kV, forming a stable Taylor cone jet
Receiving distance: 15–20 cm, controlling fibre diameter to 50–200 nm
Drum rotation speed: 300–500 rpm, achieving oriented fibre alignment
Technical Breakthroughs:
Adoption of a coaxial dual-nozzle structure to enable the preparation of Al₂O₃–SiO₂ core–shell fibres
Fibre aspect ratio > 1,000; tensile strength increased to 1.2 GPa
2. Centrifugal Spinning Process
Equipment Parameters:
Rotational speed gradient: from an initial 5,000 rpm accelerating to 30,000 rpm, with a centrifugal force field reaching 10⁴ g
Pore size design: Gradual transition from 0.2 mm at the inner ring to 0.8 mm at the outer ring, controlling the fibre diameter distribution
Vacuum drawing: Drawing ratio of 200–300 times, refining fibres to 1–3 μm
Quality control:
Fibre diameter CV value ≤ 8 per cent (measured by laser diffraction)
Slag ball content < 0.5 per cent (four-stage centrifugal slag removal)
III. Paper-based Structures: Precise Control of Vacuum Filtration and Hot-Press Curing
1. Wet-forming Process
Filter membrane configuration:
Upper layer: 0.8 μm polytetrafluoroethylene (PTFE) membrane (to trap particles >5 μm)
Lower layer: 0.2 μm aluminium oxide ceramic membrane (to control fibre interlacing density)
Vacuum control:
Staged control: -0.06 MPa (initial) → –0.09 MPa (final)
Dehydration rate: Maintained at 0.5 L/min for the first 3 minutes, followed by 0.2 L/min
Solid content gradient:
45 per cent at the bottom layer → 35 per cent at the surface layer, creating a density difference to strengthen interlayer bonding
2. Hot-press Curing Technology
Three-stage temperature ramp:
80 °C (2 hours): Removal of free water; preliminary cross-linking of the binder
150 °C (1 h): Carbonisation of the organic binder to form a carbon skeleton
280 °C (0.5 h): Melting of the inorganic binder to fill pores
Pressure curve:
Initial 1 MPa → Peak 10 MPa → Pressure held whilst cooling to 5 MPa
Stress relaxation rate < 15% (measured using a high-temperature indentation tester)
Atmosphere control:
Under N₂ protection, O₂ concentration < 50 ppm to prevent oxidation of Al₂O₃
IV. Post-treatment reinforcement: surface modification and structural enhancement
1. Atmospheric plasma treatment
Process parameters:
Power density: 0.2 W/cm², treatment time 90 s
Surface energy increase: from 45 mN/m to 75 mN/m, enhancing coating adhesion
Effect verification:
Contact angle reduced from 120° to 30° (measured using the water droplet method)
Coating bond strength increased to 8 MPa (measured using the scratch test)
2. Immersion coating technology
Coating system:
Base layer: silica sol (solid content 30%)
Top layer: aluminium oxide sol (solid content 45%)
Process control:
Coating amount: weight gain ≤ 3%
Heat treatment: Rapid curing at 500°C for 2 hours to form a gradient interface layer
3. Laser Micro-machining
Equipment parameters:
Picosecond laser: Wavelength 355 nm, pulse width 10 ps
Cutting accuracy: ±10 μm, edge heat-affected zone < 50 μm
Application scenarios:
Precision machining of irregularly shaped components (e.g. fuel cell bipolar plate flow channels)
Preparation of microporous arrays (pore diameter 50–200 μm, pore density 10⁴/cm²)
V. Quality Control: Comprehensive Inspection System
1. Microstructural Analysis
SEM observation: Fibre interlacing density ≥95 per cent, porosity <15 per cent
TEM analysis: Grain size <30 nm, α-Al₂O₃ content >98 per cent
XRD analysis: Intensity of the characteristic α-Al₂O₃ peak at 2θ = 45.8° > 90%
2. Performance Testing

3. Verification of Special Properties
Vacuum outgassing test: Total mass loss (TML) < 1.0 per cent, condensable volatile components (CVCM) < 0.1 per cent
Resistance to molten metal penetration: No signs of penetration after 30 seconds’ contact with molten iron at 1600°C
VI. Application Scenarios: The Transition from Thermal Insulation to Functionalisation
1. Aerospace
Thermal protection systems: Used in rocket engine nozzles, withstanding instantaneous temperatures of 2000°C
Electromagnetic shielding: Composite metal coating, shielding efficiency > 80 dB @ 10 GHz
2. New Energy Sector
Fuel cell separators: Double-sided CVD coating, gas tightness < 1 × 10⁻⁶ Pa·m³/s
Lithium-ion battery thermal insulation: 0.5 mm thick board, thermal runaway protection temperature > 1,000 °C
3. Semiconductor Manufacturing
Wafer carriers: Vacuum hot-press moulding, flatness ±5 μm/m²
Plasma etching chambers: Resistant to plasma corrosion, service life increased threefold
Conclusion: The ‘Material Revolution’ of Ceramic Fibre Paper
From nano-sol preparation to precision laser machining, the manufacturing processes for ceramic fibre paper have transcended the realm of traditional refractory materials, becoming a benchmark for lightweight, functionalised and precision-engineered materials. In the future, with the integration of technologies such as nanofibre self-assembly and AI-driven process optimisation, it will continue to achieve breakthroughs in the following areas:
Ultra-high-temperature insulation: Development of materials with a temperature resistance of 2,000 °C for use in nuclear fusion devices
Flexible electronics: Constructing ‘ceramic fibre paper + two-dimensional material’ composite substrates capable of withstanding over 100,000 bending cycles
Biomedical applications: Preparing biodegradable bioceramic fibre paper for use as tissue engineering scaffolds
Only by mastering core technologies such as nanoscale preparation, precision moulding and functional modification can enterprises seize the initiative in this materials revolution and propel China from being a ‘major materials producer’ to a ‘leading materials powerhouse’.